Top brand Construction
Machinery supplier
Guess you like the video
Cobalt Based Vacuum Melted Superalloys
Product Details
Longda Super alloy company’s Cobalt alloy bars FSX414, CoCrMo,X40,X45 etc are high purity, consistent quality and homogenized that satisfied to our customers home and abroad. Cobalt alloys features and properties are as follows:
• Cobalt alloys have higher melting points than nickel (or iron) alloys. This gives them the ability to absorb stress to a higher absolute temperature.
• Cobalt alloys give superior hot corrosion resistance to gas turbine atmospheres, this is due to their high chromium content.
• Cobalt alloys show superior thermal fatigue resistance and weldability over nickel alloys.
• Composition and Structure
• Cobalt alloys are termed austenitic in that the high temperature “Face Centred Cubic” phase is stabilised at room temperature. 

They are hardened by carbide precipitation, thus carbon content is critical. Chromium provides hot corrosion resistance and other refractory metals are added to give solid solution strengthening – tungsten and molybdenum – and carbide formation – tantalum, niobium, zirconium, hafnium.


Cobalt Based Super alloys

Alloy Name

UNS No.

BS NO.

AMS

Rolls-Royce

GE

Snecma

Others

CoCrMo



5384




HS21 , ASTM F75

FSX414





B50A910



X40



5382

MSRR7049 , 7122

C50TF21

DMD403.32

HS31 , PWA648

X45





B50A3748

DMD405.32


MM302







PWA657

MM509





B50TF89

DMD.401-32

PWA647



Cobalt Based Super alloys Chemical Composition

Alloy Name

AI

B

C

Nb

Co

Cr

Fe

Mn

Mo

Ni

Si

Ta

Ti

W

ZR

Others

CoCrMn



0.23


Bal

28.0


0.50

6.0


0.80






FSX414


0.100

0.25


Bal

29.5


0.7


11.0

0.90



7.0



X40



0.25


Bal

25.5


0.8


10.5

0.80



7.5



X45


0.100

0.25


Bal

25.5


0.5


10.5

0.80



7.5



MM302


0.005

0.85


Bal

21.5








10.0

0.02


MM509



0.60


Bal

23.5




10.0


3.5

0.2

7.0

0.45