				 Element  | 
			
				 Type 430  | 
		
| 
				 Carbon  | 
			
				 0.12 max.  | 
		
| 
				 Manganese  | 
			
				 1.00 max.  | 
		
| 
				 Sulfur  | 
			
				 0.030 max.  | 
		
| 
				 Phosphorus  | 
			
				 0.040 max.  | 
		
| 
				 Silicon  | 
			
				 1.00 max.  | 
		
| 
				 Chromium  | 
			
				 16.0 – 18.0  | 
		
| 
				 Nickel  | 
			
				 0.75 max.  | 
		
| 
				 Type  | 
			
				 Yield Strength 0.2% offset (KSI)  | 
			
				 Tensile Strength (KSI)  | 
			
				 % Elongation (2" Gauge length)  | 
			
				 Hardness Rockwell  | 
		
| 
				 430  | 
			
				 30 min.  | 
			
				 65 min.  | 
			
				 22 min  | 
			
				 HRB 89  | 
		
| 
				 Density (lb./ in^2) @ RT  | 
			
				 0.278  | 
		|
| 
				 Modulus of Elasticity in Tension (psi x 10^6)  | 
			
				 29.0  | 
		|
| 
				 Specific Heat (BTU/o F/lb.)  | 
			
				 32 to 212 oF  | 
			
				 0.11  | 
		
| 
				 Thermal Conductivity (BTU/hr/ft^2/ft)  | 
			
				 212oF  | 
			
				 13.8  | 
		
| 
				 932oF  | 
			
				 15.0  | 
		|
| 
				 Mean Coefficient of Thermal Expansion (in. x 10^-6 per o F)  | 
			
				 32 to 212oF  | 
			
				 5.7  | 
		
| 
				 32 to 932oF  | 
			
				 6.2  | 
		|
| 
				 Electrical Resistivity (micro ohms - cm)  | 
			
				 at 70oF  | 
			
				 60.0  | 
		
| 
				 Melting Point Range (oF)  | 
			
				 2600 - 2750  | 
		|
| 
				 Oxidation Resistance - Continuous Service(oF)  | 
			
				 1500  | 
		|