Product structure: |
|
|
Substrate: |
MOPP (uniaxially stretched polypropylene) |
|
Glue: |
Rubber-based glue |
|
Substrate color: |
Blue |
|
Features: |
|
|
It is widely attached, removes no residue |
|
|
Modified acrylic glue can be bonded with low surface energy materials and has a good bonding effect |
|
|
It can replace equivalent products (3M8898 TESA4298) |
|
|
ASTM Test Method |
|
|
Stainless steel sheet peeling force: 7.5N/ inch width |
D-3330 |
|
Tensile strength: 160 lb/inch width (700 N/ inch width) |
D-3759 |
|
Breaking elongation: 32 % |
D-3759 |
|
Total thickness 4.637mil (0.11 mm) |
D-3652 |
|
Chemical resistance test: |
||
|
Chemicals |
Appearance |
Edge soaking |
|
visualization |
Millimeter |
|
|
Isopropyl alcohol |
No change |
1 |
|
Water 48 hours |
No change |
0 |
|
PH4 |
No change |
0 |
|
PH10 |
No change |
0 |
|
Temperature resistance test: |
||
|
120 ℃ 24 hours: |
no change in visual observation |
|
|
40 ℃ 72 hours: |
||
|
Anti-moisture performance test: |
||
|
38 ℃ 24 hours 100% relative humidity: |
no change in appearance, good adhesion. |
|